Ascent Group Co., Ltd

Cross-Grade Table

Evatane EVA at a Glance

Typical property values across all five grades, CAS 24937-78-8.

Typical values, not for specification.
GradeVA %MFI (g/10 min)Density (g/cm³)Melt °CShore ATypical Application
Evatane 28-052850.9507280Film & HMA base
Evatane 28-2528250.9507175General hot melt
Evatane 40-5540550.9605550Solvent ink & foam
Evatane 33-4533450.9606263HFFR cable
Evatane 18-150181500.9408885High-speed HMA

Selection Guide

Which Grade Should You Choose

Match your process and application to the right Evatane EVA grade.

Blown & Cast Film

High cohesion and melt strength for stable bubble and clear film.

Use Evatane 28-05 →

General Packaging Hot Melt

Easy-flow grade for carton sealing and lamination.

Use Evatane 28-25 →

Solvent Adhesive & Ink

High VA for solubility and pigment binding.

Use Evatane 40-55 →

HFFR Cable & Filler

Polarity for high mineral filler loading.

Use Evatane 33-45 →

High-Speed HMA & Masterbatch

Ultra-high flow for fast coating and dispersion.

Use Evatane 18-150 →

Bitumen Modification

Flexibility and adhesion for roofing and roads.

Use Evatane 18-150 →

Need Help Deciding

Talk to Our Technical Team

Share your process and target properties; we will recommend the closest grade and supply plan.